Whole Tire Reclaim Rubber
WTR reclaim is made from end of life tyres and treads peelings. It is available in varying quality grades and smoothness. The vulcanization properties of
Swarna WTR reclaim makes it particularly suitable for a variety of natural rubber tube products. In natural tube reclaim Swarna has 4 grades
Properties: Faster mixing cycle, improved die swell, reduced power consumption due to nerve compound, no reduction in hot air ageing
properties.
Applications of Whole Tire Reclaim Rubber
- Tyres, Tread Rubber,
- Conveyor belts,
- Hot Melt Adhesives,
- Automobile components, Footwear
Particulars | Units | Standards | Highly Refined | Super Fine |
---|---|---|---|---|
Acetone Extract |
% |
ASTM D297 |
10-16 |
10-14 |
Ash |
% |
ASTM D297 |
5-9 |
8-9 |
Carbon Black |
% |
ASTM D297 |
25-30 |
25-28 |
RHC By Difference |
% |
ASTM D297 |
47 min |
40 |
Specific Gravity |
– |
ASTM D297 |
1.10 – 1.14 |
1.10 – 1.14 |
Hardness |
Shore A |
ASTM D2240 |
54– 62 |
54– 62 |
Tensile Strength |
kg/cm2 |
ASTM D412 |
40 Min |
36 |
Elongation at Break |
% |
ASTM D412 |
200 Min |
100 |
Mooney Viscosity |
ML (1+4)@100ºC. |
ASTM D1646 |
25-50 |
25-45 |
Volatile Matter |
% |
1 Max |
1 Max |
Curing | |||||||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
20min @ 140ºC | |||||||||||||||||||||||||||
WTR Reclaim |
100.00 | ||||||||||||||||||||||||||
ZnO |
5.00 | ||||||||||||||||||||||||||
Steric Acid |
2.00 | ||||||||||||||||||||||||||
MBT |
0.50 | ||||||||||||||||||||||||||
DPG |
0.20 | ||||||||||||||||||||||||||
Sulphur |
3.00 |